N2 - In this paper, we report the fatigue characteristics of IBAD/PLD YBCO coated conductors. A YBCO coated conductor used in the superconducting coil of a SMES system is repeatedly subjected to mechanical tensile or compressive strain due to the Lorentz force during electrical charging or discharging. The superconducting characteristic of this conductor may deteriorate because of this cyclic strain. Therefore, it is necessary to investigate the effect of cyclic strain on the superconducting characteristics of YBCO coated conductors that have a laminated structure. We developed an experimental apparatus with a U-shaped sample holder in order to apply cyclic strain to the sample tape. This apparatus was used to perform the fatigue tests on YBCO coated conductors in liquid nitrogen in the absence of an external magnetic field. The strain cycles with the maximum strain max (zero external strain max zero external strain) were applied and repeated up to 5000 times, and the I c measurements were performed at max. Therefore, the application of cyclic strain with max ranging from 0.3% to 0.5% did not result in any significant deterioration of the superconducting characteristics of the conductor.
AB - In this paper, we report the fatigue characteristics of IBAD/PLD YBCO coated conductors. A YBCO coated conductor used in the superconducting coil of a SMES system is repeatedly subjected to mechanical tensile or compressive strain due to the Lorentz force during electrical charging or discharging. The superconducting characteristic of this conductor may deteriorate because of this cyclic strain. Therefore, it is necessary to investigate the effect of cyclic strain on the superconducting characteristics of YBCO coated conductors that have a laminated structure. We developed an experimental apparatus with a U-shaped sample holder in order to apply cyclic strain to the sample tape. This apparatus was used to perform the fatigue tests on YBCO coated conductors in liquid nitrogen in the absence of an external magnetic field. The strain cycles with the maximum strain max (zero external strain max zero external strain) were applied and repeated up to 5000 times, and the I c measurements were performed at max. Therefore, the application of cyclic strain with max ranging from 0.3% to 0.5% did not result in any significant deterioration of the superconducting characteristics of the conductor.
UR - http://www.scopus.com/inward/record.url?scp=42149158263&partnerID=8YFLogxK
UR - http://www.scopus.com/inward/citedby.url?scp=42149158263&partnerID=8YFLogxK
U2 - 10.1088/1742-6596/97/1/012170
DO - 10.1088/1742-6596/97/1/012170
M3 - Article
AN - SCOPUS:42149158263
SN - 1742-6588
VL - 97
JO - Journal of Physics: Conference Series
JF - Journal of Physics: Conference Series
IS - 1
M1 - 012170
ER -