    Abstract

    The hydrogen embrittlement of pure titanium (Ti) and Ti-6Al-4V alloy in fluoride solution was examined by hydrogen thermal desorption analysis (TDA). The fracture surface and side surface of specimens were examined with a scanning electron microscope (SEM). Sampling was conducted at 30 s intervals and the heating rate was 100°C/h up to the terminal temperature of 800°C. The formation of sodium titanium fluoride was confirmed on the surface of Ti and Ti-6Al-4V alloy specimens that the breakdown of the protective film on the surface occurs.

    Original languageEnglish
    Title of host publicationTransactions - 7th World Biomaterials Congress
    Pages951
    Number of pages1
    Publication statusPublished - 2004
    EventTransactions - 7th World Biomaterials Congress - Sydney
    Duration: 2004 May 172004 May 21

    Other

    OtherTransactions - 7th World Biomaterials Congress
    CitySydney
    Period04/5/1704/5/21

    ASJC Scopus subject areas

    • General Engineering

    Fingerprint

    Dive into the research topics of 'Hydrogen embrittlement of Ti and Ti-6Al-4V alloy in fluoride solution'. Together they form a unique fingerprint.

    Cite this