T1 - Simultaneous fabrication of a through-glass interconnect via and a bump using dry film resist and submicron gold particles
AU - Mimatsu, Hayata
AU - Mizuno, Jun
AU - Shoji, Shuichi
AU - Kasahara, Takashi
AU - Shih, Kailing
AU - Nomura, Kazuya
AU - Kanehira, Yukio
AU - Ogashiwa, Toshinori
N1 - Copyright:
Copyright 2014 Elsevier B.V., All rights reserved.
PY - 2014
Y1 - 2014
N2 - A process for the simultaneous fabrication of through-glass interconnect vias (TGVs) and gold (Au) bumps using dry film resist and submicron Au particles is proposed. A Ti/Pt/Au layer was sputtered on the top and bottom surfaces of glass vias to improve the adhesion between the glass substrate and submicron Au particles. The submicron Au particles filled the resist holes and glass vias fabricated by photolithography and by the two-electrode method, respectively, and were then sintered. The height and diameter of the fabricated Au bumps were about 20-25 and 200 μm, respectively. The Ti/Pt/Au layer on the surface of the glass substrate was removed by Ar ion milling to isolate each bump electrically. The resistance of a single Au bump and TGV was evaluated using the four-wire ohm method to be about 0.05 Ω. Furthermore, Au bump bonding was demonstrated. Fractured Au bumps and TGVs were observed by scanning electron microscopy after the bonded sample was peeled. It is expected that this fabrication process using a dry film resist and submicron Au particles will be useful in simple packaging processes to form glass interposer substrates or glass integrated circuit chips.
AB - A process for the simultaneous fabrication of through-glass interconnect vias (TGVs) and gold (Au) bumps using dry film resist and submicron Au particles is proposed. A Ti/Pt/Au layer was sputtered on the top and bottom surfaces of glass vias to improve the adhesion between the glass substrate and submicron Au particles. The submicron Au particles filled the resist holes and glass vias fabricated by photolithography and by the two-electrode method, respectively, and were then sintered. The height and diameter of the fabricated Au bumps were about 20-25 and 200 μm, respectively. The Ti/Pt/Au layer on the surface of the glass substrate was removed by Ar ion milling to isolate each bump electrically. The resistance of a single Au bump and TGV was evaluated using the four-wire ohm method to be about 0.05 Ω. Furthermore, Au bump bonding was demonstrated. Fractured Au bumps and TGVs were observed by scanning electron microscopy after the bonded sample was peeled. It is expected that this fabrication process using a dry film resist and submicron Au particles will be useful in simple packaging processes to form glass interposer substrates or glass integrated circuit chips.
UR - http://www.scopus.com/inward/record.url?scp=84906855695&partnerID=8YFLogxK
UR - http://www.scopus.com/inward/citedby.url?scp=84906855695&partnerID=8YFLogxK
U2 - 10.1049/mnl.2014.0187
DO - 10.1049/mnl.2014.0187
M3 - Article
AN - SCOPUS:84906855695
SN - 1750-0443
VL - 9
SP - 532
EP - 535
JO - Micro and Nano Letters
JF - Micro and Nano Letters
IS - 8
ER -