抄録
The repassivation potential of corroding crevices of a duplex stainless steel was measured in a deaerated 3.5mass% NaCl solution according to JIS G 0592. The change of current density with time and preferential dissolution phase during anodic polarization in -370mV to +150mV (vs. SCE) potential region in a simulated crevice solution (25mass% NaCl, pH 0) were investigated. The repassivation potential of crevice corrosion depended on the holding potential and time for ensuring the propagation of crevice corrosion, and in all the cases, the preferential dissolution of ferritic phase was observed. The current density was rather steady during the potentiostatic measurement in the active peak region (-370mV to -260mV). While, it decreased with time in the active-passive transition region (-200mV to -150mV). In the passive region (0mV to +150mV), it first decreased, and then increased gradually. On the less-noble side of the active peak region, preferential dissolution occurred on the ferritic phase. On the other hand, on the noble side of the active peak region and in the active-passive transition region, it occurred on the austenitic phase. In the passive region, both phases dissolved evenly. These results suggest that the potential in the corroding crevice drops to the less-noble side of the active peak region by the IR drop mechanism.
本文言語 | English |
---|---|
ホスト出版物のタイトル | 17th International Corrosion Congress 2008: Corrosion Control in the Service of Society |
ページ | 927-935 |
ページ数 | 9 |
巻 | 2 |
出版ステータス | Published - 2008 |
イベント | 17th International Corrosion Congress 2008: Corrosion Control in the Service of Society - Las Vegas, NV 継続期間: 2008 10月 6 → 2008 10月 10 |
Other
Other | 17th International Corrosion Congress 2008: Corrosion Control in the Service of Society |
---|---|
City | Las Vegas, NV |
Period | 08/10/6 → 08/10/10 |
ASJC Scopus subject areas
- コロイド化学および表面化学
- 表面、皮膜および薄膜