抄録
α-Zirconium phosphate (α-ZrP) was prepared by liquid-phase deposition. Boric acid was added to a solution containing [ZrF 6] 2- anions, and phosphoric acid dropwise to cause slow decomposition of [ZrF 6] 2- and the subsequent reaction with H 3PO 4 to form α-ZrP. X-ray diffraction, scanning electron microscopy, solid-state 31P nuclear magnetic resonance spectroscopy, infrared spectroscopy, thermogravimetry, and elemental analyses indicate the formation of single-phase α-ZrP.
本文言語 | English |
---|---|
ページ(範囲) | 555-557 |
ページ数 | 3 |
ジャーナル | Chemistry Letters |
巻 | 41 |
号 | 5 |
DOI | |
出版ステータス | Published - 2012 5月 3 |
ASJC Scopus subject areas
- 化学 (全般)