抄録
Microfractographic aspects of fatigue fracture were quantitatively studied in relation to the strength of materials and stress ratios. The specimens used were heat-treated low-carbon and low alloy steels. Fatigue tests were conducted in the low- and high-cycle regions under axial load conditions. The applicability of the quantitative microfractographic data for failure analysis was pointed out.
本文言語 | English |
---|---|
ページ(範囲) | 22-27 |
ページ数 | 6 |
ジャーナル | Transactions of National Research Institute for Metals (Tokyo) |
巻 | 24 |
号 | 3 |
出版ステータス | Published - 1982 |
ASJC Scopus subject areas
- 工学(全般)