N2 - The susceptibility to delayed fracture of the alpha-beta titanium alloy Ti-6Al-4V has been investigated in acidic and neutral fluoride solutions at room temperature. The time to fracture decreased with increasing applied stress in 2.0% and 0.2% acidulated phosphate fluoride (APF) solutions at pH 5.0. The time to fracture in the 2.0% APF solution was shorter than that in the 0.2% APF solution, although at an applied stress higher than 1000 MPa, the times to fracture were almost the same in both the solutions. For immersion in the 0.2% APF solution, when the applied stress was lower than 700 MPa, delayed fracture did not occur within 1000 h. The fracture surface of specimens immersed in the 2.0% APF solution exhibited brittleness associated with hydrogen absorption, while that in the 0.2% APF solution was ductile and characterized macroscopically as having a cup-cone morphology. The amounts of hydrogen absorbed in 2.0% and 0.2% APF solutions for 24 h were approximately 200 and 30 mass ppm, respectively. As the immersion time increased, the amount of hydrogen absorbed in the 2.0% APF solution increased, whereas that in the 0.2% APF solution hardly increased. In neutral 2.0% and 0.2% NaF solutions, the delayed fracture did not occur within 1000 h, although general corrosion was observed. These results indicate that the susceptibility to delayed fracture of alpha-beta titanium alloy, compared with those of the alpha titanium and beta titanium alloy reported previously, is low in acidic and neutral fluoride solutions.
AB - The susceptibility to delayed fracture of the alpha-beta titanium alloy Ti-6Al-4V has been investigated in acidic and neutral fluoride solutions at room temperature. The time to fracture decreased with increasing applied stress in 2.0% and 0.2% acidulated phosphate fluoride (APF) solutions at pH 5.0. The time to fracture in the 2.0% APF solution was shorter than that in the 0.2% APF solution, although at an applied stress higher than 1000 MPa, the times to fracture were almost the same in both the solutions. For immersion in the 0.2% APF solution, when the applied stress was lower than 700 MPa, delayed fracture did not occur within 1000 h. The fracture surface of specimens immersed in the 2.0% APF solution exhibited brittleness associated with hydrogen absorption, while that in the 0.2% APF solution was ductile and characterized macroscopically as having a cup-cone morphology. The amounts of hydrogen absorbed in 2.0% and 0.2% APF solutions for 24 h were approximately 200 and 30 mass ppm, respectively. As the immersion time increased, the amount of hydrogen absorbed in the 2.0% APF solution increased, whereas that in the 0.2% APF solution hardly increased. In neutral 2.0% and 0.2% NaF solutions, the delayed fracture did not occur within 1000 h, although general corrosion was observed. These results indicate that the susceptibility to delayed fracture of alpha-beta titanium alloy, compared with those of the alpha titanium and beta titanium alloy reported previously, is low in acidic and neutral fluoride solutions.
KW - Corrosion
KW - Delayed fracture
KW - Fluorides
KW - Hydrogen embrittlement
KW - Ti-6Al-4V alloy
UR - http://www.scopus.com/inward/record.url?scp=14844284654&partnerID=8YFLogxK
UR - http://www.scopus.com/inward/citedby.url?scp=14844284654&partnerID=8YFLogxK
U2 - 10.1016/j.corsci.2004.08.007
DO - 10.1016/j.corsci.2004.08.007
M3 - Article
AN - SCOPUS:14844284654
SN - 0010-938X
VL - 47
SP - 1778
EP - 1793
JO - Corrosion Science
JF - Corrosion Science
IS - 7
ER -